      Cement production target vs Ball mill diameter          
                             
      1 The general sheet                
        - The sheet below gives the production in t/h of a cement mill in function of:        
          * the cement fineness target in Blaine               
          * the general dimensions of the mill              
        - The following hypotheses are used:              
          * mill in closed circuit                
          * separator of the third generation              
          * mill Length/Diameter ratio around 3,2            
          * mill speed of rotation around 73% of the critical speed          
          * filling degree of both chambers around 31%            
        - Specific power used are:                
          * 3000 Blaine: 28 kWh/t                
          * 3500 Blaine: 35,8 kWh/t                
          * 4000 Blaine: 44,4 kWh/t                
          * 4500 Blaine: 53,6 kWh/t                
        - The length of chamber 1 is defined for the coarsest cements, here 3000 up to 3500 Blaine.      
         
     
                     
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
                             
      2 Some graphics from the general sheet            
        - Speed of rotation in rpm and total length in m in function of the mill diameter in m:      
         
     
         
               
               
               
               
               
               
               
               
               
               
               
               
               
               
               
                             
        - Aborbed power in kW in function of the mill diameter in m:          
         
     
         
               
               
               
               
               
               
               
               
               
               
               
               
               
               
               
                             
        - Production in t/h at different Blaine fineness in function of the mill diameter in m:      
         
     
         
               
               
               
               
               
               
               
               
               
               
               
               
               
               
               
                             
        - First chamber specific power in kWh/t at different Blaine fineness in function of the mill diameter in m:    
         
     
         
               
               
               
               
               
               
               
               
               
               
               
               
               
               
               
                             
        - Tons of balls for 31% volume load in function of the mill diameter in m:        
         
     
         
               
               
               
               
               
               
               
               
               
               
               
               
               
               
               
                             
      3 Calculator                  
        - A quick mill sizing calculator has been developed following this presentation.        